MACOR® Machinable Glass Ceramics Corrosion Properties

Chemical Properties
Tests
Results
Solution
pH
Time
Temperature
Loss (mg/cm2)
5% HCl
00.01
24 hours
95°C
~100
.002 N HNO3
02.8
24 hours
95°C
~.6
.1 N NaHCO3
08.4
24 hours
95°C
~.3
.02 N NaCO3
10.9
06 hours
95°C
~.1
5% NaOH
13.2
06 hours
95°C
~10
H2O
07.6
24 hours
95°C
~.01
H2O
07.6
06 days
95°C
~.11