MACOR<sup>®</sup> Machinable Glass Ceramic MGC Mechanical Properties
Link to Standard Products Link to Custom Products Link to Case Studies Link to Ceramic and Glass Materials Link to Design Notes Link to Working Together Link to Accuratus Contact Form
link to Accuratus home page email link - voice: 908-213-7070 fax: 908-213-7069

Standard
Products

 

Accuflect®

MACOR®

> Fabrication

> Properties
Thermal
Mechanical
Electrical
Magnetic
Optical
Chemical

> Available Sizes

Ceramic Rod & Tube

Aluminum Nitride Substrates

 

 

MACOR® Machinable Glass Ceramic Mechanical Properties

Mechanical Properties
SI/Metric
Imperial
Density
2.52 g/cc
157 lb/ft3
Porosity
0%
0%
Young’s Modulus (25°C)
66.9 GPa
9.7x106 psi
Poisson’s Ratio
.29
.29
Shear Modulus (25°C)
25.5 GPa
3.7x106 psi
Hardness
250 Knoop 100g
48 Rockwell A
Flexural Strength
94 MPa
13,600 psi
Compressive Strength
345 MPa
50,000 psi
Fracture Toughness
1.53 MPa • m1/2
1,390 psi • in1/2
Coefficient of Kinetic Friction (25°C)
– against steel
.12
.12
against aluminum
.15
.15
against MACOR®
.15
.15
 
Macor Young's modulus and Macor flexural strength (MOR) vs temperature curves