MACOR® Machinable Glass Ceramic Electrical Properties

Electrical Properties
SI/Metric
Imperial
Dielectric Constant (25°C)
1 KHz
6.03
6.03
8.6 GHz
5.67
5.67
Loss Tangent (25°C)
1 KHz
4.7x10–3
4.7x10–3
8.6 GHz
7.1x10–3
7.1x10–3
Dielectric Strength (25°C) (.254mm)
40kV/mm
1000V/.001"
Volume Resistivity (25°C) DC
>1016 ohm • cm
>1016 ohm • cm
 
Macor Dielectric properties vs temperature curves

Back to Top

Standard Products | Custom Products and Services | Case Studies | Materials
Design Notes | Working Together | Vision | Contact Us | Site Map

1-908-213-7070

© 2013 Accuratus

Site Design M. Adams