Standard Sialon Tube Sizes

Single-Bore Cast Sialon Tube
Part
Number
Outer Diameter
Millimeters–Inches
Inner Diameter
Millimeters–Inches
500250SC
12.5mm
.500"
6.5mm
.250"
625350SC
16mm
.625"
9mm
.350"
875468SC
22mm
.875"
12mm
.468"
1125625SC
28mm
1.100"
16mm
.625"
Lengths up to 1500mm (60") are available
Tolerances
Length:   + 1.6mm (.062")
Diameter: up to 25mm (1"): + 5% or .65mm (.025") whichever is greater
  over 25mm (1"): + 4% or .65mm (.025") whichever is greater
Straightness:   .006mm/mm (.006"/inch)

Contact us with your special sizes!
 

See also: Materials > Sialon

Standard Products | Custom Products and Services | Case Studies | Materials
Design Notes | Working Together | Vision | Contact Us | Site Map

1-908-213-7070

© 2013 Accuratus

Site Design M. Adams